Abstract

Optical properties and phase transitions of (Pb1−1.5xLax)(Zr0.42Sn0.40Ti0.18)O3 (PLZST 100x/42/40/18) ceramics with different compositions have been investigated by temperature dependent spectroscopic ellipsometry. Two interband critical points (Ecp1 and Ecp2) located at about 3.9 and 5.1 eV can be obtained by fitting standard line shapes to the second derivatives of the complex dielectric functions. Based on the band-to-band transitions, the phase diagram of PLZST ceramics can be well presented. Moreover, a peculiar incommensurate antiferroelectric state has been found to exist above the temperature of the normal commensurate antiferroelectric tetragonal structure. It can be stable below Curie temperature, evolving slowly with decreasing temperature towards the commensurate structure, which is due to strong pinning of incommensurate domain walls. The phenomena can result from a competition between ferroelectric ordering and antiferroelectric ordering caused by the lanthanum modification.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.