Abstract
The failure of austenitic stainless steel during the industrial aplications is place sensitization due to heat treatment. The investigation of that failure has been investigated by researchers in particular for stainless steel 2XX and 3XX types, while there isno or little investigation for stainless steel J4 type.Furthermore, the investigation of the presence of sensitization on stainlees steel was conducted by referring to American Society for Testing and Materials (ASTM) A262-02a, which the caracterization of metal surface morphologies dan chrom content used optical microscope andscanning electron microskop, and Energy-dispersive X-ray spectroscopy, respectively. The results elucidate that sensitization is produced in temperature range from700 o C up to 900 o C .There isgrain boundaries attack onsurface morphologies after sensitization test in the temperature range from700 o C up to 900 o C ,whichis unlikely to happenat temperature of 600 o C. The possibility of chromium difusion to grain boundaries took place from the decrease of chromium content adjancent with grain boundaries and the increase of chromium content in grain boundaries, whichimplies the formation of intermetallic compound of carbide.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.