Abstract

The Virginia Department of Transportation began allowing the use of warm mix asphalt (WMA) in 2008. Although several WMA technologies were investigated prior to implementation, foamed WMA was not. This study evaluated the properties and performance of foamed WMA placed during the initial implementation of the technology to determine whether the technology had performed as expected. Six mixtures produced using plant foaming technologies and placed between 2008 and 2010 were identified and subjected to field coring and laboratory testing. Coring was performed in 2014, resulting in pavement ages from 4 to 6 years. Three comparable hot mix asphalt (HMA) mixtures were cored at 5 years for comparison. Cores were evaluated for air-void contents and permeability and were subjected to dynamic modulus, repeated load permanent deformation, and overlay testing. In addition, binder was extracted and recovered for performance grading. Similar properties were found for the WMA and HMA mixtures. One WMA mixture had high dynamic modulus and binder stiffness, but overlay testing did not indicate any tendency for premature cracking. All binders had aged between two and three performance grades above that specified at construction. WMA binders and one HMA binder aged two grades higher, and the remaining two HMA binders aged three grades higher, indicating a likely influence on aging of the reduced temperatures at which the early foamed mixtures were typically produced. Overall results indicated that foamed WMA and HMA mixtures should be expected to perform similarly.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call