Abstract

This paper intends to analyze the performance of mortars with reactive MgO, as a sustainable alternative to cement. Six different MgOs from Australia, Canada, and Spain were used in the production of mortars as partial substitutes for cement, namely 5%, 10%, 15%, 20%, and 25% (by weight). MgOs with different levels of reactivity were used to analyze its influence on the performance of MgO mortars. In order to evaluate the mechanical performance of these mortars, compressive strength, flexural strength, dynamic modulus of elasticity, and ultrasonic pulse velocity tests were performed. Compressive strength tests showed that the use of 25% reactive MgO can cause a decrease of this property of between 28% and 49%. The use of reactive MgO affected the other mechanical properties less. This paper also intends to analyze the durability performance of mortars with reactive MgO. To that effect, water absorption by capillarity was assessed. In this research, the effect of using MgO on the shrinkage was also analyzed. It was found that shrinkage may decrease by more than a half in some cases.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.