Abstract

We experimentally demonstrated a laser diode-pumped Q-switched Nd:GdTaO4 crystal laser at 1066 nm using a multilayer graphene oxide as the saturable absorber (GOSA). The GOSA is fabricated by transferring the liquid-phase-exfoliated GO nanosheets onto a K9 glass substrate. When the GOSA was inserted into the plano–plano laser cavity, a stable Q-switched laser operation is achieved with a maximum average output power of 0.382 W and repetition rate of 362 kHz. The shortest pulse duration is 194 ns and the single pulse energy is about 1.05 μJ.