Abstract
This paper introduces a parametric study of nanofiber fabrication. Poly-Caprolactone(PCL) and Chloroform are basic material for nanofiber fabrication with electrospinning method. The device for electrospinning was composed of a syringe pump, syringe, high voltage generator and 32gauge plastic nozzle. PCL concentration, applied voltage, solution flow rate and the tip to collector distance (TCD) were parameters in electrospinning method. As a result of electrospinning experiment, it was found that as TCD and applied voltage increased, the diameter of fibres was decreased. In feed rate experiment, the size of fibres decreased when feed rate decreased. The optimized PCL concentration was found at 6w/v% for the minimum of fibres.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.