Abstract
A side sealing structure including, outside a sealant, AlOx deposited using an atomic layer deposition (ALD) apparatus was employed. This structure can prevent the entry of external moisture. A liquid crystal display (LCD) with this type of structure can have long‐term high reliability as a low‐frequency driving LCD.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.