Abstract

The isothermal oxidation behavior of two TiAl alloys (as-HIP and as-RHT) were compared to explain the effect of microstructure on the oxidation resistance of TiAl alloy. After hot-pack rolling and cyclic heat treatment, the size of lamellar colonies was refined from 35.4 μm to 21.5 μm, and the β/B2 phase was effectively removed. It is concluded that the as-RHT TiAl alloy has better oxidation resistance than the as-HIP TiAl alloy. The main reason is due to refinement of lamellar colony size, elimination of β/B2 phase, uniform distribution of Nb and Mo, and the crushing of Y compounds.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.