Abstract

This study evaluates the effect of donor-doped SrTiO3 (La0.2Sr0.8Ti0.9Ni0.1O3-δ, LSTN) coating on chromia growth on the surface of porous stainless steel (STS). During subsequent exposure to wet H2 atmosphere at 800 °C, the porous STS oxidizes, and its Ohmic resistance increases slowly for 300 h to an area-specific resistance (ASR) ∼2.5 mΩ cm2, but at a much slower rate does uncoated STS and to a much lower ASR than that of uncoated STS (∼17.9 mΩ cm2). The estimated parabolic rate constant indicates that the porous LSTN-coated STS may be used at temperature <680 °C for ∼10 y.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.