Abstract
Under certain severe accident conditions, the fuel rods of nuclear power plants are exposed to high temperature/pressure steam environments in which the Zr alloy cladding is rapidly oxidized. As alternative claddings, the oxidation resistances of SiC-based materials and stainless steels with high Cr and/or Al additions have been examined from 800-1200 °C in high-pressure steam environments. Very low reaction kinetics were observed with alumina-forming FeCrAl alloys at 1200 °C while Fe-Cr alloys with only 15-20% Cr were rapidly attacked.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.