Fe 3 O 4 (FO) nanoparticles (NPs) - polyimide (PI) film was used as saturable absorber (SA), and achieved passive Q-switched output at 1.5 μm successfully. Based on the reverse saturable and saturable absorptions of FO NPs-PI film, the laser output characteristics can be further optimized by adjusting the ratio of FO NPs to PI. When the ratio of FO NPs to PI is 1:5 (FO NPs-PI (1:5)), the pulse duration and repetition rate are 0.669 μs and 5.51 kHz; this is the first time to realize the simultaneous compression of repetition rate and pulse duration. The single pulse energy and peak power are up to 364 nJ and 556 mW. The optical conversion efficiency can reach 855%, and it is about two orders of magnitude higher than other reports. The results show that it is helpful to construct high performance Q-switched pulse laser by introducing proper cavity loss through reverse saturable absorption. • Fe 3 O 4 (FO) nanoparticles (NPs) - polyimide (PI) film was used as saturable absorber (SA). • By introducing proper cavity loss through PI's reverse saturable absorption, so compression of pulse duration and repetition rate simultaneously. • Corresponding Q-switched pulsed laser performance are realized regulation and optimization by adjusting the ratio of FO NPs to PI.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.