Abstract
AbstractThe preparation process of amidoxime hollow fiber consists of three steps: (1) radiation‐induced graft polymerization of acrylonitrile (AN) onto porous hollow fiber (AN grafting), (2) chemical conversion of the cyano group into an amidoxime group (amidoximation), and (3) conditioning of the hollow fiber with alkaline solution (alkaline treatment). Systematic optimization of this preparation process was found to improve the adsorption rate. For the AN‐grafted hollow fiber having 130% degree of grafting, the optimum reaction was 1 h each for amidoximation and alkaline treatment, respectively. Also the change in the structure of the amidoxime hollow fiber with alkaline treatment was discussed based on measurements of water content, swelling and pore volume distribution, and observation of morphology of cross section by SEM.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.