AbstractAluminum nitride (AlN) ceramic substrates have been fabricated using non‐aqueous tape casting and pressureless densification under flowing N2 atmosphere. Considering the economic and environmental impact, a new strategy of solvent and dispersant system was adopted to prepare AlN slurries with high solid loading. According to the viscosity characteristics of AlN slurries, dispersant content was adjusted to be 0.5 wt% of AlN powder in order to optimize the rheological behavior of AlN slurries. The addition contents of binder and plasticizer were both optimized as 5 wt% of AlN powders by combining the viscosity of slurries and tensile strength of green tapes. Green AlN tapes were fabricated with an optimized tape casting process such as dry temperature. The exclusion process of organic additives was investigated by employing thermogravimetric analysis. Flat and dense AlN ceramic substrates with a relative bulk density over 99.75 % were achieved after being sintered under 1800°C for 6 hours, which had a maximum size of 110 × 110 mm. The thermal conductivity of the AlN substrate could reach 145 Wm−1K−1.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.