Abstract

The optimization of recovery of copper from Akiri hematite-dominated copper ore using hydrometallurgy was investigated in this study. The Akiri copper ore deposit hosts a high-grade copper mineral from which copper metal can be extracted. However, the ore is dominated by gangue minerals that need to be mechanically reduced for efficient copper recovery. The purpose of this study is to optimize the extraction of the metal from hematite-dominated copper ore. The experiments that were carried out in the course of this study include crushing, pulverization,mineralogical and chemical characterizations of the sample and sulpheric acid leaching. Response surface methodology was used to optimize the system parameters namely;temperature, concentration of the leachant and contact time so that an efficient method will be developed for the extraction of copper.Chalcopyrite, covellite and cuprite are the copper minerals while the gangues minerals were quartz ,mica, hematite,etc.on the characterization of the copper ore. The major oxides in the ore are hematite ,copper oxide and silica and revealed that the ore contains 4.61% copper and 65.8% iron. Effect of three independent factors like concentration ,temperature and contact time for copper extraction from the hematite-dominated copper ore was studied.Central composite design method was applied to the proposed quadratic model that connect the factors used for best copper extraction at the best process condition. The work shows that concentration of the acid was the best efficient factor for copper extraction compare to temperature and contact time. This may be as a result of high value of F-statistics for the concentration of the leachant, which effects to high level of copper extraction.Experimental and predicted values for weight loss from the copper ore were obtained as 39.10% and 39.03% at optimum conditions, respectively. The optimum conditions of 1.5M acid concentration, 90oC reaction temperature and 90minutes contact time were obtained and from which 6.64%Cu at recovery of 92.0% and 2.31%Fe was obtained without stirring. Also, the ore was subjected to leaching with stirring at 400rpm with the optimum conditions obtained to know the effect. The grade obtained was 7.84% Cu at recovery of 83.51% and iron content 5.47%. This shows that leaching without stirring is the best option against leaching with stirring to extract the copper and to reduce the iron and other gangues contents in the copper ore.The activation energies were estimated as 13.20kJ/mol and 22.67kJ/mol for liquid film diffusion and diffusion product layer respectively, the values indicate that the leaching rate is controlled by diffusion process.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call