Abstract
A frequent problem encountered by photoresists during the manufacturing of semiconductor device is that activating radiation is reflected back into the photoresist by the substrate. So, it is necessary that the light reflection is reduced from the substrate. One approach to reduce the light reflection is the use of bottom anti-reflective coating (BARC) applied to the substrate beneath the photoresist layer. The BARC technology has been utilized for a few years to minimize the reflectivity. As the chip size is reduced to sub 100nm, the photoresist thickness has to decrease with the aspect ratio being less than 3.0. Therefore, new Organic BARC is strongly required which has the minimum reflectivity with thinner BARC thickness and higher etch selectivity toward resists. Hynix Semiconductor Inc., Nissan Chemical Industries, Ltd., and Brewer Science, Inc. have developed the advanced Organic BARC for achieving the above purpose. As a result, the suitable high performance 248nm Organic BARCs, NCA series, were achieved. Using CF4 gas as etchant, the plasma etch rate of NCA series is about 1.4 times higher than that of conventional 248nm resists. NCA series can be minimizing the substrate reflectivity at below 45nm BARC thickness. NCA series show the excellent litho performance and coating property on real device.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have