Abstract

In order to optimize the loading of 3-(1,1-dicyanothenyl)-1-phenyl-4, 5-dihydro-1H-pryazole (DCNP) in polyetherketone (PEK-c) guest-host polymer films, ten kinds of DCNP/PEK-c thin films, in which the weight per cent of DCNP changes from 5 to 50, were prepared. Their second-order nonlinear optical coefficients χ33(2) at λ = 1064 nm were measured by using Maker fringe method after poling under the optimal poling condition. Their optical waveguide transmission losses were measured at 632.8 nm. Optimal weight per cent of the chromophore for the DCNP/PEK-c guest-host polymer system has been determined as about 20 for use in the integrated optical devices.