We demonstrate three-dimensional optical confinement in CdTe-based microcavities. While the vertical confinement is determined by epitaxially grown CdMnTe/CdMgTe Bragg mirrors, the lateral confinement is achieved by defining pillar structures with electron beam lithography and reactive ion etching. The optical confinement is shown by a size-dependent energy splitting between the fundamental and higher photonic modes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.