The heteronuclearΜ-oxoacetate with the composition [Fe2NiO(CH2COO)6(H2O)3]·2H2O decomposed on heating, forming nickel ferrite NiFe2O4 and (depending on the decomposition conditions) in part other solid phases. H2O, CH3COOH, acetone and CO2 were also formed in the decomposition. A reaction scheme is given for the decomposition. The products were porous powders with grain diameters between 3 and 10Μm. On increase of the temperature of decomposition from 300 to 800 ‡C, the BET surface area and the surface area of the pores decreased, but only a small alteration in grain size was observed. As a result of thermal treatment in the temperature region abone 800‡C, larger aggregates of grains were formed in sintering processes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.