Abstract

The process of selective laser melting (SLM) of an Al-Si-Mg-Cu powder composite with the addition of quasicrystal reinforcements under conditions of a limited powder amount was investigated. The morphology and microhardness of the obtained scan single tracks were discussed, and the optimal sintering parameters were found to be in the Linear Energy Density (LED) range 0.21-0.30 J/mm. The following SLM parameters: P = 370 W and v = 1650 mm/s given the optimal characteristics of scan single tracks geometry with less defects. The obtained composites exhibited an improved hardness with the highest values of 235 HV with the 8% of reinforcements in the powder mixture.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.