The article is devoted to the impact of carbon additives on densification and mechanical properties of ZrC/C heteromodulus composites. In case of addition of small amount of carbon to ZrC residual porosity decreases, whereas higher carbon content leads to more than 3vol.% increase in residual porosity. Moreover, increase in carbon content in ZrC/C composites boosts toughness of sintered materials. For example, КIC=4.3 MPa×m1/2 for ZrC and КIC=7 MPa×m1/2. for 3 vol.% C. For 15 vol.% of C, toughness is the lowest and equals 5.3 MPa×m1/2. The extrapolation of the dependence of toughness on the non-porous state of materials is КIC0=13.2 MPa×m1/2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.