We observed how PFPE lubricant film formed to magnetic disk surface using AFM with a fluoride coated probe. We found that PFPE lubricant did not uniformly cover the carbon protective surface but concentrated in valleys of surface roughness. The lubricant film has one to two step structure and the first step height is almost the same as the radius of molecular gyration. After the pin-on-disk test, the lubricant step height and the coverage increased, compared to the initial state.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.