Abstract

This paper presents the results of laser welding of dissimilar joints, where low-carbon and stainless steels were welded inthe lap joint configuration. Performed welding of austenitic and ferritic-pearlitic steels included a sealed joint, where only partial penetration of lower material was obtained.The authors presented acomparative study of the joints under different configurations. The welding parameters for the assumed penetration were estimated via anumericalsimulation. Moreover, a stress–strain analysis was performed based on theestablished model. Numerical analysis showed significant differences in joint properties, therefore, further study was conducted. Investigation of the fusion mechanism in the obtained joints wascarried out using electron dispersive spectroscopy (EDS) and metallurgical analysis. The study of the lap joint under different configurations showed considerable dissimilarities in stress–strain distribution and relevant differences in the fusion zone structure. The results showed advantages of using stainless steel as the upper material of a microstructure, and uniform chemical element distribution and stress analysis is considered.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.