Area-Selective Atomic Layer Deposition, AS-ALD, can be initiated by local area-activation1,2 or -deactivation.3 We studied the maskless growth of ZnO from diethyl zinc and water. The method is based on the different nucleation delays that arise from precursor adsorption on OH-terminated versus that on H-terminated Si-substrate. TEOS (tetraethyl orthosilicate) and H2O were used to deposit a SiO2 seed layer by EBID (e-beam-induced deposition) in a pattern of 500x500 nm2 dots on H-terminated a-Si:H substrate. After this local activation the substrate was coated with a ZnO film in a conventional ALD reactor using 80 cycles of diethyl zinc and water vapor. In situ spectroscopic ellipsometry (Fig. 1), SEM, cross-sectional TEM and energy dispersive X-ray spectroscopy (EDX) showed good areal selectivity with ZnO growth only occurring on the SiO2 dots. This observation was corroborated by Density functional theory calculations suggesting a kinetically hindered surface reaction between diethyl zinc and H-terminated Si. Atomic Layer Etching, ALE, was also tested on a ZnO case. Current ALE technology is emerging in both thermal, isotropic and plasma-based, anisotropic approaches.4 In this presentation we will demonstrate a plasma-assisted ALE-process driven by radicals, and therefore being isotropic. The ALE-process was tested at temperatures between 150 and 250 °C. We used alternating doses of acetylacetone (Hacac) and O2-plasma intermitted by Ar-purging. The ZnO-layer thickness as measured by spectroscopic ellipsometry decreased linearly with the number of cycles. In a synergy test, we proved that only the alternated dosing of Hacac and O2-plasma caused ZnO etching, whereas Hacac and O2-plasma alone did not (Fig. 2). Preliminary infrared studies suggest that Hacac forms volatile complexes by metal oxide surface chelation (e.g. Zn(acac)2), whereas the O2-plasma step removes non-reactive Hacac fragments to refresh the surface for the next etching cycle.5 TEM- and XPS-inspection indicated no damage of the ZnO surface, good preservation of the ZnO-stoichiometry throughout the etching process, and no distinct contamination. Furthermore, we demonstrated this ALE-process to be selective over SiO2. We believe that this novel plasma-assisted ALE-concept can be extended to several other materials. [1] A. J. M. Mackus et al., Nanoscale, 4, 4477 (2012). [2] R. Chen et al., Adv. Mater., 18, 1086 (2006). [3] A. Mameli et al., Chem. Mater. 29, 921 (2017). [4] D. R. Zywotko, et al., Chem. Mater. 29, 1183 (2017). [5] M. A. George, et al., J. Electrochem. Soc., 143, 3257 (1996). Figure 1
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have