Abstract
A series of phosphorus‐containing copolyesters was prepared by polycondensation of 2‐(6‐oxido‐6H‐dibenzo<c,e><1,2>oxaphosphorin‐6‐yl)1,4‐benzenediol, 1 , or of an equimoleculare amount of 1 and different bisphenols 2 , such as: hydroquinone, 4,4′‐(hexafluoroisopropylidene)diphenol, 4,4′‐isopropylidenediphenol, 4,4′‐(1,4‐phenylene‐diisopropylidene)bisphenol, 2,7‐dihydroxynaphthalene, 4,4′‐dihydroxybiphenyl, 9,9‐bis‐(p‐hydroxyphenyl)fluorene, with an aromatic diacid chloride containing two preformed ester groups 3 , namely terephthaloyl‐bis‐(4‐oxybenzoyl‐chloride). The copolyesters exhibited thermal stability having the decomposition temperature above 350°C and char yield at 700°C in the range of 19–41%. The glass transition temperature was in the range of 131–164°C. Some of the polymers exhibited thermotropic liquid crystalline behavior.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.