Abstract
In order to determine the weldability of a new type of low alloy high strength steel, the feasibility of the proposed welding process was examined and the welding procedure qualification of a new type of ultrahigh strength steel WELDOX 1100 was carried out through the weldability test of the welded joint, the small iron research and the highest hardness test. . The test result satisfies the specification requirements and proves that the proposed welding process plan is correct and feasible. It provides a reliable basis for the preparation of welding process documents and ensures the smooth development of the company's new products.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.