Using total yield photoelectron spectroscopy we demonstrate that the room temperature (RT) hydrogenation of amorphous germanium (a-Ge) surfaces leads to the creation of a deep defect band 0.45 eV above Ev that anneals out at ≈ 300°C. We argue that this defect is related to the high concentration of hydrogen at the growth surface and is responsible for the high surface defect density (≈ 1018 cm−3) in g.d. a-Ge:H and a-Si:H as derived from yield and PDS measurements. We show that the surface defect density in g.d. a-Si:H can be reduced through hydrogen dilution and through post-deposition anneals but not through post-hydrogenation. Drawing from the analogy with c-Si we propose that a small fraction (≈ 10−4) of hydrogen in the bond center position is responsible for the observed defect which is different from the more common dangling bond defect.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.