Anode-free (or lithium-metal-free) batteries with garnet-type solid-state electrolytes are considered a promising path in the development of safe and high-energy-density batteries. However, their practical implementation has been hindered by the internal strain that arises from the repeated plating and stripping of lithium metal at the interlayer between the solid electrolyte and negative electrode. Herein, we utilize the titanium nitrate nanotube architecture and a silver-carbon interlayer to mitigate the anisotropic stress caused by the recurring formation of lithium deposition layers during the cycling process. The mixed ionic-electronic conducting nature of the titanium nitrate nanotubes effectively accommodates the entry of reduced Li into its free volume space via interfacial diffusion creep, achieving near-strain-free operation with nearly tenfold volume suppressing capability compared to a conventional Cu anode counterpart during the lithiation process. Notably, the fabricated Li6.4La3Zr1.7Ta0.3O12 (LLZTO)-based initial-anode-free quasi-solid-state battery full cell, coupled with an ionic liquid catholyte infused high voltage LiNi0.33Co0.33Mn0.33O2-based cathode with an areal capacity of 3.2 mA cm−2, exhibits remarkable room temperature (25 °C) cyclability of over 600 cycles at 1 mA cm−2 with an average coulombic efficiency of 99.8%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.