Pure lead germanate (LG), 0.1 wt% Nd+3 doped (LG.1Nd+3) and 0.2wt% Nd+3 doped (LG.2Nd+3) lead germanate single crystals were grown by controlled cooling of melt. Room temperature pyroelectric coefficient p(T) was found to increase with doping. In LG.1Nd+3 doping enhances p(T) and figure of merit and there by increases the applicability of lead germanate as a pyroelectric detector.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.