Abstract
The deformation behaviour of diamond-like carbon (DLC) coatings on silicon substrates induced by indentation has been investigated. DLC coatings, deposited by a plasma-assisted chemical vapour deposition technique, were subjected to nanoindentation over a range of maximum loads from 100 mN to 300 mN. The resulting load-displacement plots displayed pop-ins for maximum loads of 200 mN and above, with no distinct pop-out for any of the loads studied. Compressive deformation of the coating, up to a strain of ∼ 9%, was observed. The coating–substrate composite was devoid of cracks at lower loads, but at the maximum load of 300 mN, ring cracks in the coating and a median crack in the substrate were observed. Furthermore, cracking, {111} slip and localized phase transformations were observed in the silicon substrate. The onset of these structural changes was correlated to the mechanical behaviour during indentation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.