Abstract
AbstractWe present a micromechanical characterization of shales from the Horn River Basin, NW Canada. The shales have contrasting mineralogy and microstructures and play different geomechanical roles in the field: the sample set covers an unconventional gas reservoir and the overburden unit that serves as the upper fracture barrier. Composition and texture were characterized using X‐ray diffraction, mercury injection porosimetry, and scanning electron microscopy (SEM). Grid nanoindentation testing was used to obtain the mechanical response of the dominant phases in the shale microstructure. Samples were indented parallel and perpendicular to the bedding plane to assess mechanical anisotropy. Chemical analysis of the grids with SEM‐EDS (energy dispersive X‐ray spectroscopy) was undertaken and the coupled chemo‐mechanical data was used in a statistical clustering procedure (Gaussian mixture model) to reveal the mechanical properties of each phase. The results show that the overburden consists of a soft clay matrix with highly anisotropic elastic stiffness, and stiffer but effectively isotropic inclusions of quartz and feldspar; the significant anisotropy of the overburden has been previously observed on a much larger scale using microseismic data. Creep displacement is concentrated in the clay matrix, which is the key phase for fracture barrier and seal applications. The reservoir units are harder and have more isotropic mechanical responses, primarily due to their lower clay content. Despite varied compositions and microstructures, the major phases of these shales (clay/organic matrix, quartz/feldspar, dolomite, and calcite) have unique mechanical signatures, which will aid identification in future micromechanical characterizations and facilitate their use in upscaling schemes.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.