Abstract
An atomic force microscope (AFM), with a specially prepared diamond tip, has been modified to measure indentation hardness with an indentation depth as low as 1 nm. This indentation depth is much smaller than the depth of more than 20 nm that have been reported to date. The AFM indentation technique allows the hardness measurements of surface monolayers and ultrathin films in multilayered structures at very shallow depths and low loads. The nanoindentation hardness of single crystal silicon is measured using this technique. A subtraction technique is also described which allows the actual hardness measurements of rough surfaces such as magnetic thin film rigid disks.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.