Self-powered energy harvesting technologies have been intensively investigated by employ- ing Pb-free piezoelectric materials. One such Pb-free piezoelectric material, the ceramic 0.97(Na0.5K0.5)NbO3-0.03(Bi0.5Na0.5)TiO3, was prepared by employing the conventional mixed oxide method. 0.97(Na0.5K0.5)NbO3-0.03(Bi0.5Na0.5)TiO3 ceramics were prepared and the effect of sintering temperature on the microstructure, piezoelectric and ferroelectric properties were system- atically investigated for energy harvesting applications. The crystal structure of 0.97(Na0.5K0.5)NbO3- 0.03(Bi0.5Na0.5) TiO3 Pb-free piezoelectric ceramics, sintered at temperatures between 1080 °C and 1160 °C, was examined by X-ray diffraction analysis. The dielectric properties of 0.97(Na0.5K0.5)NbO3-0.03(Bi0.5Na0.5)TiO3 ceramics were measured from 1 kHz to 1 MHz for the various sintering temperatures. We expect that optimization of sintering parameters can improve the piezoelectric and ferroelectric properties of 0.97 (Na0.5K0.5)NbO3-0.03(Bi0.5Na0.5)TiO3 ceramics for energy harvesting.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call