The formation of cobalt-nitride thin films by the ion reacting deposition method was investigated. A low energy broad-beam ion source (Kaufman type) was used for ionizing nitrogen. From the X-ray diffraction spectra, it was found that the N-rich cobalt-nitrides, Co3N and Co2N, were formed only under the deposition condition of low ion current density. The magnetic properties of the films changed suddenly with increasing Jion. Hc took a maximum value at Jion=1.5 (mA/m2)/(Å/s), above which the N-poor composition, Co4N, was formed. The nitrogen, which was contained in the films but did not take part in the nitriding reaction, was degassed above 250°C

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.