本文对拜耳法赤泥进行改质后制备出一种铁水预处理脱硅脱磷剂,在其熔化性能测定的基础上,进行了铁水预处理脱硅脱磷高温模拟实验研究。研究结果表明:在赤泥中适量加入CaO进行改质,可显著降低赤泥的熔点,提高其熔化速度。利用赤泥与CaO质量比为100:30的赤泥基脱硅脱磷剂进行铁水预处理,铁水脱硅率达到98.2%,脱磷率达到75.5%,脱硅脱磷效果显著。 A novel desilication and dephosphorization agent for hot metal pretreatment was designed and developed by the chemical modification of Bayer red mud. According to the determination results of melting properties for the red mud-based desilication and dephosphorization agent, the simulation experiment of the hot metal pretreatment was carried out at high temperature, and the results were shown as follows. The melting properties of the red mud-based desilication and dephosphorization agent could be improved remarkably by a proper addition of CaO. The red mud-based desilication and dephosphorization agent with the mass ratio of 100:30 for red mud and CaO was used in the simulation experiment process of the hot metal pretreatment. The desilication ratio and the dephosphorization ratio in the hot metal reached 98.2% and 75.5%, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.