Abstract

To realize a large-scale consumption of red mud in the steelmaking industry, a new recycling method was investigated through the pre-reduction roasting experiment and the slag-metal interaction experiment simulating the hot metal pretreatment process in the steelmaking industry. In virtue of the sensible heating of the hot metal and the reducibility of [C] and [Si], the iron could be separated and recovered from the pre-reduced red mud pellets into the hot metal directly with a recovery rate exceeding 75%. With the composition adjustment of the residual oxides in the pre-reduced red mud (PRRD) using CaO and Al2O3 or aluminium dross (AD), a slag having a low melting point (below 1300 °C) and a high sulfide capacity (lgCS = −2.3) was formed, and more than 94% of [S] in the hot metal could be removed into this slag through the slag-metal interaction. The desulfurization efficiency of the flux (PRRD-CaO–Al2O3; PRRD-CaO–AD) is approximate to the traditional desulfurizing flux (CaO–CaF2). The advantages of this method are summarized as the low energy cost and the slag valorization.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call