As a part of precision finishing of ceramics for circuit components, forsterite is lapped with 6-12μ diamond abrasives using a rotary disc type lapping tester concerning lapping quantity, lapping force and surface roughness with discussions on lapping mechanism from abrasive numbers acting simultaneously and scratching force. The results obtained are as follows : (1) The influence of lapping speed is greater on lapping quantity and surface roughness than that of lapping pressure, leading to the smaller effect of depth of cut in abrasive grains. (2) Numbers of abrasives acting simultaneously are calculated as about 1/500-1/1000 of those of ideally distributed ones. (3) Lapping force is derived from the sum of scratching and ploughing forces as 73-280g, which is considerably approximate to the empirical one.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.