Abstract

AbstractNatural rubber (NR), polyurethane rubber (PUR), and NR/PUR‐based nanocomposites were produced from the related latices by adding a pristine synthetic layered silicate (LS; sodium fluorohectorite) in 10 parts per hundred parts rubber (phr). The dispersion of the LS latices in the composite was studied by X‐ray diffraction (XRD) and transmission electron microscopy (TEM). Further information on the rubber/LS interaction was received from Fourier transform infrared spectroscopy (FTIR) and dynamic mechanical thermal analysis (DMTA). Tensile and tear tests were used to characterize the performance of the rubber nanocomposites. It was found that LS is more compatible and thus better intercalated by PUR than by NR. Further, LS was preferably located in the PUR phase in the blends, which exhibited excellent mechanical properties despite the incompatibility between NR and PUR. Nano‐reinforcement was best reflected in stiffness‐ and strength‐related properties of the rubber composites. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 543–551, 2004

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.