Conditions in a single pore of a battery plate were simulated by using a cadmium chip of millimeter dimensions covered with an electrolyte film of micron thickness. In situ microscopy was applied to study changes in the electrode morphology during charge and discharge. Passivation and increases in particle sizes due to precipitation and electrodeposition of dissolved cadmium species were found to cause profound loss in electrode capacity on repeated charge and discharge.