A flexible poly(dimethyl siloxane) diacrylate (PDMSDA) crosslinker was synthesized using different molecular weights of poly(dimethyl siloxane) (PDMS, M n =550, 1,700, 4,000 g/mol). The monodisperse polystyrene (PS) particles crosslinked with various contents of PDMSDA were prepared by dispersion polymerization, and applied as seed particles in the seeded polymerization. The crosslinking density of the PS particles was determined from the rate of transport of the monomer molecules to the crosslinked seed particles. It was confirmed that the monomer swelling capacity of seed particles and final morphological changes of polymer beads were determined significantly by the crosslinking density of the seed particles. In addition, the morphological change was not observed without the oligomer swelling step in the seeded polymerization due to the hydrophobic property of PDMS. When highly crosslinked seed particles were used in the seeded polymerization, peculiar morphology (doublet structure) of polymer beads appeared.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.