Abstract

A unique mechanism based on extensive field and laboratory studies is presented to account for certain premature failures of flexible pavements in cold areas like those in Scandinavia and in northern parts of Canada and the United States. Water condensing at the interface between pavement and granular base accumulates at subzero temperatures resulting in excess moisture in this zone. During the thaw period of the uppermost base layer, the excess water in the aggregate is trapped between impervious layers of frozen ground to the sides and below as well as an impervious layer of asphalt pavement above. Because of this containment, high pore water pressures can occur, leading to loss in shear strength of the base material and thus to failure of the pavement structure itself. It was found that under special conditions, excess moisture can accumulate in granular base with a silt content greater than 20 percent and very high pore water pressures can develop during initial thaw at the pavement-soil interface. With silt contents of less than 2 percent, excess pore water pressures can be avoided during thaw. It was also shown that when a clean open gravel is placed below the pavement on top of a silty base material, moisture accumulation near the pavement-base interface can be prevented, and thus also the development of high pore water pressures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.