Abstract

The modes of grain selection in spiral selector were investigated by both a ProCAST simulation and experimental confirmation. The results show that the efficiency of grain selection in starter block is associated with the geometry shape. At the early stage of grain selection, the optimization of grain orientation is dominated by competitive grain growth, but the optimization of grain orientation in starter block is gradually dominated by geometry shape at the later stage of grain selection. Besides, the spiral part could also optimize the orientation of the selected single crystal when the initial angle is large enough, and the single crystal selection in spiral parts with different pitch lengths and initial angles is dominated by different modes. The simulation results agree well with experimental ones.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.