Abstract
The competitive growth of columnar grains in a single-grain selector, which is used for directional solidification of single-crystal blades from nickel-based superalloys, has been investigated by electron back-scattered diffraction and local X-ray diffraction analysis. It has been found that the competitive grain growth in a starter block is determined by the crystallographic factor: rapidly growing grains with the axial orientation close to the [001] direction dominate in this part of the casting. For the competitive grain growth in a helicoidal separator, the geometric factor (the position of a grain at the input of the separator) is also important. The results obtained suggest that an appropriate geometry of the single-grain selector was chosen. In addition, the distribution of the orientations of columnar grains obtained by electron backscattered diffraction, can be used for approximate estimation of the yield of suitable (i.e., with the deviation of the axial orientation from the [001] direction within a specified tolerance) single-crystal blades.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.