Abstract
A method for determining the level of interfacial stresses in single-crystal nickel superalloys and the results of its determination are presented. The splitting of the (h00) X-ray diffraction peaks in the X-ray diffraction patterns of the γ and γ′ phases that is caused by interfacial thermal stresses is studied.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.