Abstract

The mineral processing experimental research was carried out on the hematite bearing characteristics of low grade, fine grain,complex composition. The results showed that using the technological flowsheet of “stage grinding- low intensity magnetic separation”, the iron concentrate with recovery of 36.56% and grade of 65.85% Fe can be obtained. And the iron concentrate with recovery of 17.23% and grade of 63.53% Fe can be obtained by “stage grinding-HIMS process-reverse flotation” process. The final iron concentrate with TFe grade of 65.10%,yield of 19.19% and total iron recovery of 53.79% from the raw ores with TFe grade of 23.41% was obtained, with the first stage grinding size being 55% -0.074mm and the second stage,93% -0.074mm.