Abstract

Apparently C-doped and undoped or pure nanoparticles of anatase were synthesized using a microwave hydrothermal process in the temperature range of 140–180°C for 1h from several Ti precursors, such as Ti ethoxide, Ti isopropoxide and Ti oxysulfate. Nanoparticles of anatase samples were characterized by powder X-ray diffraction, transmission electron microscopy (TEM) and photocatalytic activity measurements. Results showed that nanoparticles in the size range of 4–17nm of anatase were obtained in all cases with surface areas in the range of 151–267m2/g. The photocatalytic activity of the prepared titanias was measured using methylene blue (MB) and NOx molecules. Because MB has very strong adsorption on the samples, photocatalytic degradation under either solar light or black light irradiation was found to be very limited. However, the DeNOx abilities of carbon-doped titanias were higher than those of Degussa P25 commercial titania sample and undoped or pure titanias especially under irradiation by long wavelength or visible light (>500nm).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.