Abstract

Effects of various finish rolling temperatures on the microstructure, texture, mechanical properties and stretch formability of rolled and annealed Mg-3Al-0.5Ca-0.2Gd (wt%) alloy were investigated in this paper, and it was found that compared with grain size and second phase particles, the basal textures, tensile properties and stretch formability Mg-3Al-0.5Ca-0.2Gd alloy are more sensitive to the increasing finishing rolling temperature. For the rolled and annealed Mg-3Al-0.5Ca-0.2Gd alloy, their grains barely grow up and second phase particles are slightly coarsened, while their basal poles are obviously weakened and tilted with increasing finish rolling temperature. Consequently, the weakened and RD-tilted basal textures are beneficial to the gradually improved elongation and stretch formability of Mg-3Al-0.5Ca-0.2Gd alloy. It is investigated that the gradually activated non-basal slips, e. g. 〈c 〉, 〈c + a〉 dislocations due to the increasing finish rolling temperature could contribute to the weakened RD-tilted textures in rolled and annealed Mg-3Al-0.5Ca-0.2Gd alloy.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.