Abstract

ABSTRACT The influences of Mn level (0–0.8 wt%) on the microstructure and mechanical properties of as-cast and T6 heat-treated low-silicon cast aluminium alloys were investigated. The results indicated that the addition of 0.5% Mn completely transformed the needle-like β-Fe phase in as-cast condition into a small-sized π-Fe phase, and the π-Fe phase was fully dissolved after T6 heat treatment. The as-cast and T6 heat-treated alloys with 0.5% Mn achieved the best combination of strength and ductility. However, an excess addition of Mn reduced the mechanical properties due to the occurrence of coarse π-Fe phase (as-cast state), α-Al(Fe, Mn)Si phase (T6 heat-treated state) and eutectic Si. With the increase of Mn content from 0 to 0.8%, the fracture modes of the as-cast alloys changed from intergranular + cleavage fracture to intergranular + quasi-cleavage fracture; The fracture modes of the T6 heat-treated alloys underwent a transition from intergranular + cleavage fracture to quasi-cleavage fracture and then to intergranular + cleavage fracture.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.