Abstract

Aluminium metal matrix composites reinforced with TiO2 were synthesized using powder metallurgy route. The compositions such as Al-2.5%TiO2, Al-5%TiO2, Al-7.5%TiO2 and Al-10%TiO2 were milled using ball mill for 1 hour. The green compacts were prepared using 400 kN hydraulic press. The sintering was done by using electric muffle furnace at a temperature of 550°C for 1 hour. Hot extrusion was carried out for the sintered composite samples with suitable punch and die. The mechanical properties such as ultimate tensile strength, yield strength, percentage elongation and hardness have been studied for the hot extruded samples. The microstructures of the extruded composites were analyzed using optical microscope and reported. The high compressive strength was obtained for the Al-5%TiO2 composite.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.