ZrB2–SiC ceramic composites were prepared through water-based gelcasting and pressureless sintering. Effects of the pressureless sintering temperature (1500–2000°C), heating rate (5–15°C/min) and soaking time (0.5–2h) on the relative density, microstructure and mechanical properties of the ZrB2–SiC composites were investigated in detail. A sintering temperature of 2000°C, a heating rate of 5°C/min and a soaking time of 2h were found to be the optimal pressureless sintering procedure. The relative density, flexural strength and fracture toughness of the ZrB2–SiC composite prepared under the optimum condition were 97.8%, 403.1±27.8MPa and 4.05±0.42MPa·m1/2, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.