Abstract

Three different sintered ZnO ceramics were prepared by magnetic pulsed compaction (MPC) and other conventional methods. The microstructures of the sintered ZnO ceramics prepared by MPC at sintering temperatures ranging from 900 to 1300°C showed a homogeneous grain growth compared to those of the samples prepared using other methods under the same sintering conditions. This implies that interpowders and/or intergrains can induce the minimization of wall friction effect because of the application of a high compaction pressure for a short process time in the MPC method. In addition, the microstructure of the sample obtained using the cold isostatic pressing method showed the presence of heterogeneous regions, indicating its low quality even though the densities of the three different samples were almost similar in the range of 97–99% at sintering temperatures of 900, 1100, and 1300°C. Therefore, different methods used for the compaction of ZnO ceramics may result in different microstructural and physical properties of the product.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.